Effect of additions of CrB2, TіВ2 and wc on the structure formation in the diamond-Fe-Cu-Ni-Sn system: formation, properties, application

Authors

  • В. А. Мечник Інститут надтвердих матеріалів ім. В.М. Бакуля

Keywords:

diamond, iron, copper, nickel, tin, chromium diboride, titanium diboride transition zone, phase, composite, decarburization, pressure, temperature, structure, properties, wear resistance

Abstract

Oneffect of CrB2, TiB2 and WC the formation of the micro- and nanostructures in the composite diamond-Fe-Cu-Ni-Sn sintered in molds in a muffle furnace with subsequent hot pressing are investigated. The mechanisms that contribute to the improvement of mechanical properties of such composites depending on their production technology have been elucidated.

 

 

Author Biography

  • В. А. Мечник, Інститут надтвердих матеріалів ім. В.М. Бакуля
    с.н.с.

Published

2017-07-28

How to Cite

Effect of additions of CrB2, TіВ2 and wc on the structure formation in the diamond-Fe-Cu-Ni-Sn system: formation, properties, application. (2017). Journal of Surface Physics and Engineering, 11(4), 378-392. https://periodicals.karazin.ua/pse/article/view/8945